Part II · The Equipment · Family 4 · Control It · Stage 2 · First month

Piping, Fittings, Flanges, and Gaskets

Pipe carries every fluid between the machines the other chapters cover, and its joints are where most leaks start. What a line is made of, how it is joined, and what its gasket and bolts can take decide whether your repair holds.

Lessons and simulators

Lessons teach one thing step by step. Simulators are free play: best after the lesson.

What kills it

Normal numbers

Maker’s values override these.

PointTypical
Seawater velocity in 90/10 Cu-Ni≤ 3 m/s
Galvanized steel, hot fresh waterBelow about 60 °C — above it the zinc stops protecting
GRP pipeUp to about 80 °C; resin maker's figure
PVC drain and sanitaryBelow about 60 °C; no steam
Flange faces before boltingParallel within about 1 mm; holes line up without bars
Socket-weld gap at receptacle bottomAbout 1.5 mm
Bolt thread past the nut1–3 full threads
Flange torqueStar pattern, 30 % · 60 % · 100 %, then once round at 100 %
Hydrotest after repair, pressure pipingTypically 1.5 × design, held while every joint is walked
Support spacing, steel, water-filled (shore guide; ships closer)DN25 ~2 m · DN50 ~3 m · DN100 ~4 m

Reading the gauges

Each one is a set of readings. Decide what they mean and what you’d check first, then look.

Symptoms

SymptomCheck firstLikely causesAction
Pinhole on a seawater bend or just downstream of a valveWall at the outside of the bendErosion — velocity, throttling, high-speed GS pumpingClamp; renew the spool; pump in low speed
Rust stain or wet patch on laggingStrip the lagging thereCorrosion under wet insulationUT the wall; renew pipe; re-lag dry
Steel bolts thin and scaly on a Cu-Ni or bronze flangeBolt materialGalvanic — steel is the anodeStainless or bronze bolts; insulating kit where specified
Small-bore line cracked at a fitting near an engineSupport near the teeVibration fatigueSupport it or fit a hose; renew the fitting
Flange leaks after a new gasket, worse hotFaces parallel? Gasket type?Pulled in by bolts; wrong gasket for the heat; not re-torquedRealign; right gasket; retorque cold
Heater flange leaks on a cold start, stops warmHow fast steam went onGasket relaxed while cold; thermal shockWarm through slowly; renew if it repeats
Cast-iron flange cracked at a bolt holePartner flange faceRaised face on flat face; over-torquedFull-face gasket; cast-iron torque; replace
Threaded joint leaks through more sealantThread formsNPT on BSPT; parallel thread without a washerMatch parts; washer or O-ring
Compression fitting weeps; tightening doesn't cure itTube bottomed? Ferrule brand?Not bottomed; mixed makers; over-tightenedNew ferrule, tube cut square and bottomed
Bellows bulging or weepingTie rods; alignment; lengthInner ply failed; thrust on flanges; misalignedNip up for tonight; replace; fit the rods
Pressure on a "dead" line, pumps stoppedBoundary valves; drain crackedValve letting by; trapped pressure; sea headThird valve; bleed; watch it stay at zero
Pipe springs when a flange is brokenSupports either sideUnsupported run; strain locked in at fit-upSupport; refit without forcing
New spare won't fit — holes or bolt circle wrongStamps on both flangesDifferent standard or ratingAdapter spool; drill only where class allows
Air system losing pressure fast, compressors stoppedRate of fall; soapy waterFitting and hose leaks; drain traps passingFix the leaks before blaming the compressor

Draft: this page is drawn from the book manuscript and is still being checked.