Constant current at the charger’s limit until the voltage reaches the boost setting, then the current tapers off at constant voltage, then back to float.
Float is the voltage the charger holds the bank at forever: just enough to replace self-discharge. About 2.25 V per cell for flooded cells (13.5 V a 12 V block) and 2.27 V for VRLA at 25°C: 27.0 and 27.2 V on a 12-cell bank. A NiCd bank is different: about 1.4 V a cell, 19 or 20 cells, 27 to 28 V on a 24 V bank. Set the charger for the bank in front of you.
Boost (2.35 to 2.40 V per cell) recharges quickly after a discharge, and equalizes a flooded bank. Hours, not weeks. Many VRLA makers don’t allow it at all.
Temperature: the right voltage falls by about 3 mV per cell for every degree warmer. 36 mV per degree on a 24 V bank. A hot battery room on a fixed float voltage overcharges; a cold one undercharges.
Too low and the plates sulfate: the bank loses capacity quietly. Too high and it gases and loses water (flooded) or dries out and can run away thermally (VRLA).
| Per cell, 25°C | Flooded | VRLA |
|---|---|---|
| Float | 2.25 V | 2.27 V |
| Boost | 2.40 V | 2.35 V* |
| Full, at rest | 2.12 V | 2.15 V |
| Discharged | 1.75 V | 1.75 V |
*only if the maker allows. Typical figures; use the values on the battery label and in the charger manual.